Comparative Evaluation of Solubilities of Two Nanohybrid Composite Resins in Saliva Substitute and Distilled Water: An in vitro Study

Pranjal S Walzade, Sumanthini MV, Vanitha U Shenoy, Rohini P Mahajan

Citation Information : Walzade PS, MV S, U Shenoy V, Mahajan RP. Comparative Evaluation of Solubilities of Two Nanohybrid Composite Resins in Saliva Substitute and Distilled Water: An in vitro Study. J Contemp Dent 2017; 7 (2):82-85.

DOI: 10.5005/jp-journals-10031-1190

License: CC BY 3.0

Published Online: 01-12-2013

Copyright Statement:  Copyright © 2017; The Author(s).


Abstract

Aim of the study

To determine the solubility of nanohybrid (NH) composite resins when immersed in saliva substitute and distilled water.

Materials and methods

A total of 60 disc-shaped samples (n = 30) were prepared in teflon molds of diameter 10 mm × 2 mm thickness from two NH composite resins. They were light-cured following which the samples were removed and weighed three times using a digital balance. Samples were then immersed in test solutions, i.e., 100 mL of distilled water and saliva substitute each stored for 24 hours and 7, 14, 21, and 28 days in an incubator at 37°C at 100% humidity. At the time intervals mentioned, the samples were removed from the incubator, washed with distilled water, blotted dry, and weighed. Samples were again immersed in fresh test solutions. Difference in preweight and postweight of samples was calculated and data were analyzed using appropriate test by testing normality. A p-value < 0.05 was considered to be significant.

Results

The results were analyzed using one-way analysis of variance (ANOVA). As observed from the baseline weight to the 28th day weight, there was a loss of weight of the samples in all the groups except NH composite resin (Flash) in distilled water.

Conclusion

From the results of the study, it was observed that there was no statistically significant difference in weight, with respect to the solubility of the two NH composite resins and the two solutions tested. Clinical significance of the study is that the NH composite resin that shows lesser solubility can be the choice for an esthetic restorative material in patients for long-term results.

How to cite this article

Mahajan RP, Shenoy VU, Sumanthini MV, Walzade PS. Comparative Evaluation of Solubilities of Two Nanohybrid Composite Resins in Saliva Substitute and Distilled Water: An in vitro Study. J Contemp Dent 2017;7(2):82-85.


HTML PDF Share
  1. Effects of staining and bleaching on color change of dental composite resins. J Prosthet Dent 2006 Feb;95(2):137-142.
  2. Color stability and degree of cure of direct composite restoratives after accelerated aging. Oper Dent 2007 Jul-Aug;32(4):406-411.
  3. Nano-composite dental resins: an overview. Ann Dent Specialty 2015 Apr-Jun;3(2):52-55.
  4. Evaluation of weight change in three different light cured composite restorative materials stored in water: an in vitro study. J Conserv Dent 2008 Jul-Sep;11(3):108-111.
  5. Influence of ketones on selected mechanical properties of resin composites. J Dent Res 1992 Nov;71(11):1847-1850.
  6. Hygroscopic and hydrolytic effects in dental polymer networks. Dent Mater 2006 Mar;22(3):211-222.
  7. Hygroscopic expansion and solubility of composite restoratives. Dent Mater 2003 Mar;19(2):77-86.
  8. The influence of short and medium-term water immersion on the hydrolytic stability of novel low-shrink dental composites. Dent Mater 2005 Sep;21(9):852-863.
  9. Evaluation of the effect of surface polishing, oral beverages and food colorants on color stability and surface roughness of nanocomposite resins. J Int Oral Health 2015 Jul;7(7):63-70.
  10. Curing-light intensity and depth of cure of resin-based composites tested according to international standards. J Am Dent Assoc 2002 Apr;133(4):429-434.
  11. Resin-based composites. J Am Dent Assoc 2003 Apr;134(4):510-512.
  12. Alternative interpretations of water sorption values of composite resins. J Dent Res 1985 Jan;64(1):78-80.
  13. Evaluation of the effect of water on three different light cured composite restorative materials stored in water: an in vitro study. Int J Dent 2012 Oct;2012:640942.
  14. Sorption and solubility of different light-activated composites. Int Dent Afr Ed 2012;3(1):32-38.
  15. Characterization of water sorption, solubility and filler particles of light-cured composite resins. Braz Dent J 2009 Jan;20(4):314-318.
  16. The weight change of various light-cured restorative materials stored in water. J Contemp Dent Pract 2005 May;6(2):72-79.
  17. Relationship between the degree of conversion, solubility and salivary sorption of a hybrid and a nanofilled resin composite. J Appl Oral Sci 2008 Mar-Apr;16(2):161-166.
  18. ; Heymann, H.; Swift, EJ.; Sturdevant, CM. Sturdevant's art and science of operative dentistry. 6th ed. St. Louis (MO): Mosby; 2006. p. 519-520.
PDF Share
PDF Share

© Jaypee Brothers Medical Publishers (P) LTD.